      鋁卷生產(chǎn)注意事項(xiàng)

      來(lái)源:http://163888.com.cn/ 發(fā)布時(shí)間:2021-11-10

      一、氣條和夾渣
      1、 Air bar and slag inclusion
      在鑄軋上可能產(chǎn)生的原因:生產(chǎn)工藝沒(méi)嚴(yán)格執(zhí)行(精煉不到位)、爐外除氣不到位(除氣箱漏氣)、鋁水處理不到位、過(guò)濾作用不明顯、空氣濕氣太重。
      Possible reasons for casting and rolling: the production process is not strictly implemented (refining is not in place), the degassing outside the furnace is not in place (gas leakage in the degassing box), the aluminum water treatment is not in place, the filtering effect is not obvious, and the air moisture is too heavy.
      整改措施:進(jìn)行一次性投料、按操作工藝撒覆蓋劑、加強(qiáng)精煉、解決除氣箱漏氣問(wèn)題、鋁水處理干凈、增加過(guò)濾裝置保證鋁水經(jīng)過(guò)過(guò)濾。
      Rectification measures: conduct one-time feeding, sprinkle covering agent according to the operation process, strengthen refining, solve the problem of air leakage in the degassing box, clean the aluminum water, and add a filtering device to ensure that the aluminum water is filtered.
      二、長(zhǎng)條狀小裂口
      2、 Elongated small fissure
      鑄軋上可能產(chǎn)生的原因:咀皮損壞或損傷
      Possible causes on roll casting: nozzle skin damage or damage
      整改措施:咀皮存在以上問(wèn)題立刻斷板,保證生產(chǎn)時(shí)咀皮完好。
      Rectification measures: if the nozzle skin has the above problems, the plate shall be broken immediately to ensure that the nozzle skin is intact during production.
      鋁板生產(chǎn)廠家
      三、黑條
      3、 Black bar
      鑄軋上可能存在的問(wèn)題:工藝沒(méi)有執(zhí)行到位,鋁水處理不好。
      Possible problems in casting and rolling: the process is not implemented in place and the aluminum water treatment is not good.
      整改措施:制定生產(chǎn)工藝,加強(qiáng)鋁水處理。
      Rectification measures: formulate production process and strengthen aluminum water treatment.
      四、擦劃傷
      4、 Scratch
      鑄軋可能產(chǎn)生的原因:剪板機(jī)下臺(tái)面磨擦鋁板表面造成。
      Possible causes of casting and rolling: the lower table surface of the shear rubs against the surface of the aluminum plate.
      整改措施:對(duì)剪板機(jī)下臺(tái)面進(jìn)行整改。
      Rectification measures: rectify the lower table of the plate shear.

      丁香花在线观看免费观看图片_国产亚洲精品无码成人_久久久久国产精品_国产精品精华液网站

        <ol id="jaitn"><optgroup id="jaitn"></optgroup></ol>
        <center id="jaitn"></center>

        <samp id="jaitn"><acronym id="jaitn"></acronym></samp>
        <center id="jaitn"></center>